24/11/2024

High Shrink Ratio Polyolefin
Art.-No. 911-01536 | HFT-333-PO-BK Details

Application Ideal for providing insulation of electrical connections, terminals, components and wiring systems. Requires a minimum shrink temperature of 120 °C and is well suited to manual as well as automatic methods of application. Suitable for use as a continuous insulation sleeve in a variety of industrial applications e.g aerospace, military and railway industries.
Colour Black (BK)
Description HEATSHRINK HFT 6.0/2mm BLACK
Material Polyolefin (PO)
PART DESCRIPTION HFT-333-PO-BK
Part No. HFT62TBK
Product Family HFT-333 High Flexible
Product Group High Shrink Ratio Polyolefin
Shrink Ratio 3:1
Type HFT-333
Recov. ∅ d max. 2.0mm
Supplied ∅ D min. 6.0mm
Wall (WT) 0.65mm
Dielectric Strength 20kV/mm
Dielectric Strength test method ASTM D2671
Elongation at break 500%
Intermittent Operating Temperature +225°C
Min. Shrink Temperature - °C +100 °C
Operating Temperature -55 °C to +135 °C
Tensile Strength 18MPa
GTIN-13 / EAN 6005242011481